04-28-2015, 10:57 AM
You guys just described why I like to taper the shaft and the hole that it fits. It's easy to control by sneaking up on the fit with a file. When it assembles about 3/4 of the way, it's time for heat and glue. Try a practice piece and see for yourself sometime.
Btw, Loctite 680 is just a thicker 609 to me. It stays put better. If you heat things up too hot it will smoke on assembly but seems to work anyway. Spit sizzle hot and a little more seems to be just right. It melts at 250C (480F) and will re-fuse when cooled. I don't see anything to be concerned with.
Btw, Loctite 680 is just a thicker 609 to me. It stays put better. If you heat things up too hot it will smoke on assembly but seems to work anyway. Spit sizzle hot and a little more seems to be just right. It melts at 250C (480F) and will re-fuse when cooled. I don't see anything to be concerned with.