01-26-2022, 04:07 PM
Those are blow holes. Too wet moulding sand, poor porosity, and/or too low metal temp. Ask me how I know......
Precision Matthews High Precision Mill Vise
|
« Next Oldest | Next Newest »
|
Messages In This Thread |
Precision Matthews High Precision Mill Vise - by EdK - 01-22-2022, 02:50 PM
RE: Precision Matthews High Precision Mill Vise - by Highpower - 01-22-2022, 05:17 PM
RE: Precision Matthews High Precision Mill Vise - by EdK - 01-22-2022, 06:33 PM
RE: Precision Matthews High Precision Mill Vise - by Mayhem - 01-22-2022, 07:44 PM
RE: Precision Matthews High Precision Mill Vise - by EdK - 01-24-2022, 12:29 PM
RE: Precision Matthews High Precision Mill Vise - by Highpower - 01-24-2022, 08:08 PM
RE: Precision Matthews High Precision Mill Vise - by EdK - 01-24-2022, 10:37 PM
RE: Precision Matthews High Precision Mill Vise - by rleete - 01-25-2022, 08:07 AM
RE: Precision Matthews High Precision Mill Vise - by EdK - 01-25-2022, 11:01 AM
RE: Precision Matthews High Precision Mill Vise - by vtsteam - 01-26-2022, 04:07 PM
|