Redrying Conditions - Non-Low Hydrogen Stick Electrodes
Stick Electrode
Electrode Group
Final Redrying Temperature
Time
E6010: Fleetweld 5P, 5P+
E6011: Fleetweld 35, 35LS, 180
E7010-A1: SA-85(1)
E7010-G: SA-HYP+(1)
E8010-G: SA-70+(1), SA-80(1)
E9010-G: SA-90(1)
Fast Freeze - excessive moisture is indicated by a noisy arc and high spatter, rusty core wire at the holder end or objectionable coating blisters while welding.
Re-baking of this group of stick electrodes is not recommended.
Not Recommended
Stick Electrode
Electrode Group
Final Redrying Temperature
Time
E6010: Fleetweld 5P, 5P+
E6011: Fleetweld 35, 35LS, 180
E7010-A1: SA-85(1)
E7010-G: SA-HYP+(1)
E8010-G: SA-70+(1), SA-80(1)
E9010-G: SA-90(1)
Fast Freeze - excessive moisture is indicated by a noisy arc and high spatter, rusty core wire at the holder end or objectionable coating blisters while welding.
Re-baking of this group of stick electrodes is not recommended.
Not Recommended