My local welding shop always seems to be out of what I'm looking for -- ER70S-2 or ER70-6 so I get the other. They say one flows better in the puddle due to more of some alloying agent, but honestly, I can't detect much of a difference.
Drycleaning coathangers are fine to get up to experiment with -- just make sure you get the paint off first. They're a little thicker in diameter than 1/16" TIG filler rod, so your puddle will be a little chunkier.