12-19-2015, 04:32 PM
(12-19-2015, 10:37 AM)RobWilson. Wrote:(12-19-2015, 09:44 AM)Dr Stan Wrote: I'll have to respectfully disagree as grinding the weld flush re-hardens the weld thus requiring a second round of annealing.
Here's a good YouTube on how to resistance weld a bandsaw blade including a 2nd tempering/annealing step.
https://www.youtube.com/watch?v=GBwr3oPJHcs
With respect could you please explain how grinding the blade heats the blade up to a sufficient temperature that it becomes hardened ?
Rob
All one needs to do is watch the color change of the blade and then refer to a steel color/temp chart. You'll quickly discover just how hot the blade becomes during grinding which in turn explains the re-hardening.