11-17-2015, 08:03 PM
(11-17-2015, 07:29 PM)EdK Wrote:(11-17-2015, 07:24 PM)wrustle Wrote: By the way Ed..............what is this HSS you mention?????
I suspected you'd be using aluminum specific inserts with sharp tips.
Ed
Actually Ed, the tip is a .03" radius. the chip breaker itself is razor sharp, and that is what gets the material to "peel" off in a steady strand that can be directed by the coolant flow into the bed of the machine instead of wrapping around either the part or the spindle.
Best Regards,
Russ
Check us out on Facebook and give us a "Like"
Crosby Machine Company, Inc
Russ
Check us out on Facebook and give us a "Like"
Crosby Machine Company, Inc