I have read that too Greg. I used weld mesh to line the inside of the container I use and a chunk of flat plate on the bottom. I figured that was line of sight enough but I am not sure that it really makes all that much difference, as the top surface always cleans up as well as the bottom. Sometimes I need to cycle a part through a couple of times but I think that is dependent upon the state in which I found them. I also give them a (very) quick scrub with some hot water when I fish them out.
I think the one thing that the molasses method has over this one is that you can throw all the parts in at once, where you would likely have to do individual parts or a few smaller parts at a time. I think electrolysis would still be quicker in the long run
I think the one thing that the molasses method has over this one is that you can throw all the parts in at once, where you would likely have to do individual parts or a few smaller parts at a time. I think electrolysis would still be quicker in the long run