(08-15-2014, 12:18 PM)oldgoaly Wrote: DA
Got a question for you, what is running after you turn the flame off? air compressor? Did you add a little ferrosilicone or is it ferrosilicate? to the iron or is that only when fired in a cupola? Thanks for posting the videos! tt
probably the blower, but what you hear may also be from the Thomas Air pump that I use which is a heck of lot quitter then an air compressor.
and yes I add Silicon to the melt just before pouring to help with graphite formation, sometimes it works sometimes it doesn't.
here's a short clip from today of me preheating the furnace in prep for melting CI
Will post the video of the pour this evening.
The other half
DA
dallen, proud to be a member of MetalworkingFun Forum since Apr 2012.